Chemical resistance testing exposes a cured coating to a named chemical for a set time and records what happens to the film. There is no single rating. The result is a list: which chemical, how strong, how long, and what effect.

No coating resists everything. Chemical resistance testing shows which substances a cured film withstands, at what strength, and for how long.

What the test measures

The test records the effect of a liquid on a cured coating after a set period of contact. The effects looked for are blistering, softening, swelling, discolouration, loss of gloss and loss of adhesion.

How the test is carried out

The methods are in ISO 2812, which has several parts. They differ in how the liquid meets the film.

Method How the chemical is applied What it represents
Immersion The coated panel stands in the liquid. Tanks, bunds and surfaces that stay wet with the chemical.
Absorbent medium A pad soaked in the liquid is laid on the film and covered. A spill left to sit.
Spotting Drops of the liquid are placed on the film. Splashes and drips.

After the set time the panel is cleaned and examined, and often examined again after a recovery period. Some effects, such as softening, reverse once the liquid has gone.

How to read the result

A chemical resistance result always has four parts.

  • The chemical. Named exactly. "Acid" is not a result. "Sulphuric acid" is.
  • The concentration. A coating that withstands a 10% solution may not withstand the concentrate.
  • The contact time. One hour, 24 hours and seven days are different tests.
  • The outcome. No effect, staining only, softening, or failure.

Read the outcome with care. Staining is a change in appearance. The film may still be intact and protecting the surface. Blistering and loss of adhesion mean the film has failed.

What it means in use

Match the test to the exposure. A garage floor sees splashes of oil, fuel and brake fluid that are wiped up. A spotting or short-contact result describes that. A bund that holds a spill for days needs an immersion result.

Whatever the result, a spill that is cleaned up promptly does less damage than one left to sit.

What the result does not tell you

There is no universal chemical resistance rating, so results from different makers are hard to compare unless the chemical, strength and time all match.

Tests are run at room temperature unless stated. Heat speeds up chemical attack. Hot liquids, and steam cleaning, are harsher than the test.

Mixtures behave differently from their ingredients. A cleaning product is not the same as the acid or alkali it contains.

Results apply to a fully cured film. A coating exposed to chemicals before it has cured, at the time its data sheet gives, will not perform as tested.

A chemical that is not on the list has not been tested. It is not safe to assume the result.

On our product pages

Where a product has been tested, its page shows the result, the method and, where the method has one, the rating. Results published on this site come from internal testing to the stated method. They are given for technical reference and comparison.

If a figure you need is not shown, ask our technical team.

Leave a comment

Please note, comments need to be approved before they are published.

This site is protected by hCaptcha and the hCaptcha Privacy Policy and Terms of Service apply.

Latest Stories

This section doesn’t currently include any content. Add content to this section using the sidebar.